The first phase consists of gravitational separation to remove the heavy impurities and ... batches were prepared by wet-mixing, drying, pressing (semi-dry press) and fired at temperatures from 1000 to 1350 °C. The ... microstructure of traditional triaxial porcelain (kaolin- ite-quartz-feldspar) bodies have been studied in great. Get Price